A superalloy is a kind of metal material based on iron, nickel, and cobalt, which can work at high temperatures above 600℃ and under certain stress for a long time. It has excellent high-temperature strength, good oxidation resistance and thermal corrosion resistance, good fatigue performance, fracture toughness, and other comprehensive properties, and is also known as "superalloy". Spherical Superalloy Powder is usually used in 3D printing.

Please contact us if you need customized services. We will contact you with the price and availability in 24 hours.

Product Product Code Purity Size Contact Us
Spherical Superalloy Powder3D-Superalloy-CU-PO1Customize0-15μm
Spherical Superalloy Powder3D-Superalloy-CU-PO2Customize15-53μm
Spherical Superalloy Powder3D-Superalloy-CU-PO3Customize45-105μm
Spherical Superalloy Powder3D-Superalloy-CU-PO4Customize75-150μm
Spherical Superalloy Powder3D-Superalloy-CU-PO5CustomizeCustomize

Spherical Superalloy Powder Particle Size

0-15μm, 5-25μm, 15-45μm, 15-53μm, 45-75μm, 45-105μm, 75-150μm. (Various granularities can be customized according to customer requirements)


Spherical Superalloy Powder Grade

GradeChemical CompositionParticle Size Distribution
ElementsInpurities
IN625(GH3625)        Cr: 20.0-23.0
        Mo: 8.0-10.0
        Nb: 3.15-4.15
        Fe: ≤5.0
        Si: ≤0.50
        Ni: Bal           
 Ti: ≤0.40              
        Al: ≤0.40                         C: ≤0.10                        Co: ≤1.00         S: ≤0.015             P: ≤0.015 Y: ≤0.005          
        15-45μm    
        15-53μm    
        53-120μm  
        53-150μm  
IN718(GH4169)        Ni: 50.0-55.0
        Cr: 17.0-21.0
        Nb: 4.75-5.25
        Mo: 2.80-3.30
        Ti: 0.65-1.15
        Al: 0.20-0.80
        Cu: ≤0.30
        Ni: Bal
      O: ≤0.01          15-45μm  
        15-53μm  
        53-120μm
        53-150μm 
IN713(K418)        Cr: 11.5-13.5
        Mo: 3.8-4.8
        Al: 5.5-6.4
        Ti: 0.5-1.0
        Nb: 1.8-2.5
        N: Bal  
        C: 0.08-0.16    
        Fe: ≤1.0    
        O: ≤0.01      
        15-45μm  
        15-53μm  
        53-120μm
        53-150μm 
IN939        Cr: 22.0-22.8  
        Co: 18.5-19.5  
        W: 1.8-2.2
        Nb: 1.8-2.5  
        Ta: 1.3-1.5
        Ti: 3.6-3.8
        Al: 1.8-2.0
        Zr: 0.05-1.4
        Ni: Bal
        C: 0.13-0.17    
        B: 0.004-0.012  
        N: ≤0.001
        S: ≤0.001
        Pb: ≤0.001
        Bi: ≤0.001
        Ag: ≤0.001
        O: ≤0.01     
        15-45μm  
        15-53μm  
        53-120μm
        53-150μm 
IN738LC        Cr: 14.0-16.0
        Co: 8.0-9.00
        Ti: 2.50-4.00
        Al: 2.50-4.00
        Mo: 1.00-2.00
        W: 2.00-3.00
        Ni: Bal        
        Ta: 1.00-2.00
        Nb: 0.50-1.50
        C: ≤0.15
        Fe: ≤0.10
        Zr: ≤0.10
        B: ≤0.15
        O: ≤0.01
        15-45μm  
        15-53μm  
        53-120μm
        53-150μm 


Spherical Superalloy Powder Particle Size Description

● 0-15μm (D10=3~5μm, D50=6~10μm, D90=12~14μm)

● 5-25μm (D10=5~10μm, D50=15~20μm, D90=20~25μm)

● 15-45μm (D10=15~20μm, D50=25~30μm, D90=35~40μm)

● 15-53μm (D10=15~20μm, D50=25~35μm, D90=45~50μm)

● 45-75μm (D10=45~55μm, D50=55~65μm, D90=70~75μm)

● 45-105μm (D10=50~60μm, D50=75~85μm, D90=95~105μm)

● 45-150μm (D10=55~70μm, D50=110~120μm, D90=140~150μm)

● 75-150μm (D10=80~90μm, D50=110~125μm, D90=135~150μm)

Spherical Superalloy Powder Series

Spherical Superalloy Powder Series


Spherical Superalloy Powder Application

Aerospace field, energy field


Spherical Superalloy Powder Applicable processes

Laser/electron beam additive manufacturing (SLM/EBM, 3D printing)

Direct laser deposition (DLD)

Powder hot isostatic pressing (HIP)

Metal injection molding (MIM)

Powder metallurgy (PM)

Laser cladding (LC), etc.


Packing of Spherical Superalloy Powder

Standard Packing:

Typical bulk packaging includes palletized plastic 5 gallon/25 kg. pails, fiber and steel drums to 1 ton super sacks in full container (FCL) or truck load (T/L) quantities. Research and sample quantities and hygroscopic, oxidizing or other air sensitive materials may be packaged under argon or vacuum. Solutions are packaged in polypropylene, plastic or glass jars up to palletized 440 gallon liquid totes Special package is available on request.

E FORUs’Spherical Superalloy Powder is carefully handled to minimize damage during storage and transportation and to preserve the quality of our products in their original condition.

Related Products
+ 1 (212)5181387
+ 1 (212)5181387